Oda Kiichi
Yoshio Tetsuo
O-oka Kazuo
Abstract
A series of ferroelectric glass-ceramics was elaborated by the controlled growth of Ba(1-x)Sr(x)TiO(3) crystal particles in the glass system 60[Ba(1-y)Sr(y)]TiO(3)-10Al(2)O(3)-30SiO(2)(0≦y≦0.2) in molar basis. Analysis of crystal phases by X-ray diffraction revealed that Sr content in Ba(1-x)Sr(x)TiO(3) increased with increasing content of SrO in glasses by its preferential transfer into the crystal phase, and the appropriate temperature for the crystal growth was 1100°C. Curie temperatures of glass -ceramics shifted to lower temperature with increasing SrO content in the crystal and comparatively high dielectric constant was obtained at room temperature for a glass-ceramics with y=0.2. Frequency dependences of dielectric constant and loss tangent were examined in the frequency range from 1 K to 1 M Hz.
Publication Title
Memoirs of the School of Engineering, Okayama University
Published Date
1983-02-25
Volume
volume17
Issue
issue1
Publisher
岡山大学工学部
Publisher Alternative
School of Engineering, Okayama University
Start Page
97
End Page
105
ISSN
0475-0071
NCID
AA00733903
Content Type
Departmental Bulletin Paper
OAI-PMH Set
岡山大学
language
English
File Version
publisher
NAID
Eprints Journal Name
mfe