ID | 32855 |
JaLCDOI | |
フルテキストURL | |
著者 |
Shimamura, Yasunori
Departments of Orthopaedic Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Kaken ID
publons
Nishida, Keiichiro
Departments of Orthopaedic Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Kaken ID
publons
researchmap
Imatani, Junya
Department of Orthopaedic Surgery, Okayama Saiseikai General Hospital
Noda, Tomoyuki
Departments of Orthopaedic Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
ORCID
Kaken ID
publons
Hashizume, Hiroyuki
Department of Orthopaedic Surgery, Kasaoka Daiichi Hospital
Ohtsuka, Aiji
Human Morphology, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Kaken ID
publons
researchmap
Ozaki, Toshifumi
Departments of Orthopaedic Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Kaken ID
publons
researchmap
|
抄録 | We biomechanically evaluated the bone fixation rigidity of an ONI plate (Group I) during fixation of experimentally created transcondylar humerus fractures in cadaveric elbows, which are the most frequently observed humeral fractures in the elderly, and compared it with the rigidity achieved by 3 conventional fixation methods:an LCP reconstruction plate 3.5 using a locking mechanism (Group II), a conventional reconstruction plate 3.5 (CRP) with a cannulated cancellous screw (Group III), and a CRP with 2 cannulated cancellous screws (CS) in a crisscross orientation (Group IV). In the axial loading test, the mean failure loads were:Group I, 98.9+/-32.6;Group II, 108.5+/-27.2;Group III, 50.0+/-7.5;and Group IV, 34.5+/-12.2 (N). Group I fixations failed at a significantly higher load than those of Groups III and IV (p0.05). In the extension loading test, the mean failure loads were:Group I, 34.0+/-12.4;Group II, 51.0+/-14.8;Group III, 19.3+/-6.0;and Group IV, 14.7+/-3.1 (N). Group IV fixations showed a significantly lower failure load than those of Group I (p0.05). The fixation rigidities against mechanical loading by the ONI plate and LCP plate were comparable. These results suggested that an ONI system might be superior to the CRP and CS method, and comparable to the LCP method in terms of fixation rigidity for distal humerus fractures. |
キーワード | distal humerus
fracture
biomechanics
internal fixation
elderly
|
Amo Type | Original Article
|
出版物タイトル |
Acta Medica Okayama
|
発行日 | 2010-04
|
巻 | 64巻
|
号 | 2号
|
出版者 | Okayama University Medical School
|
開始ページ | 115
|
終了ページ | 120
|
ISSN | 0386-300X
|
NCID | AA00508441
|
資料タイプ |
学術雑誌論文
|
言語 |
英語
|
論文のバージョン | publisher
|
査読 |
有り
|
PubMed ID | |
Web of Science KeyUT |